Welcome to Jiangsu DLX alloy Co., Ltd.

Email:sales8@dlx-alloy.com Mobile/Whatsapp:+86 199 0611 9641

Specialized manufacturer of high temperature alloys, precision alloys and Incoloy,over 20 years.

Contact Us
tel

Whatsapp:+86 199 0611 9641

Email:sales8@dlx-alloy.com

Add:NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu,China

Placement:Home>>High Temperature Strip>>Element

High Temperature Strip

A-286 (UNS S66286) Iron-Based Superalloy Strip High-Strength Fasteners & Turbine Components
A-286 (UNS S66286) Iron-Based Superalloy Strip High-Strength Fasteners & Turbine Components

A-286 (UNS S66286) Iron-Based Superalloy Strip High-Strength Fasteners & Turbine Components

Product Details

A-286 Alloy Strip Banner

Introduction to A-286 Alloy Strip

A-286 (UNS S66286) is a high-performance, iron-based superalloy strip known for its excellent high-temperature strength, corrosion resistance, and creep resistance. This precipitation-hardened alloy is widely used in industries like aerospace, gas turbines, and energy, where mechanical components are exposed to extreme conditions. It's particularly essential for manufacturing high-strength fasteners, turbine components, and exhaust systems.

Key Properties of A-286 Alloy Strip

A-286 alloy strip offers a balanced combination of mechanical properties that make it suitable for various high-performance applications:

  • High Tensile Strength – Retains strength at elevated temperatures (up to 1300°F / 700°C).

  • Excellent Creep Resistance – Maintains performance under prolonged stress and high temperatures.

  • Superior Oxidation & Corrosion Resistance – Prevents scaling and degradation in harsh environments.

  • Age-Hardenable – Can be further strengthened via heat treatment (solution annealing + aging).

  • Machinability & Weldability – Easier to process compared to other nickel-based superalloys.

A-286 Alloy Strip details

A-286 Alloy Strip comparison

Comparison Parameter Table

Item

A-286

Nimonic80A

Nimonic 90

GH1140

GH3625

GH3536

GH4169

C

≤0.08

≤0.1

≤0.13

0.06-0.12

≤0.1

0.05-0.15

≤0.08

Mn

≤2

≤1

≤1

≤0.7

3.14-4.15

--

≤0.35

Fe

rest

≤3

≤1.5

rest

≤0.5

--

rest

P

≤0.04

≤0.02

--

≤0.025

--

--

--

S

≤0.03

≤0.015

≤0.015

≤0.015

--

--

≤0.01

Si

≤1

≤1

≤1

≤0.8

--

--

≤0.35

Cu

--

--

≤0.2

--

--

--

≤0.3

Ni

24-27

rest

--

35-40

rest

rest

50-55

Co

--

≤2

15-21

--

≤1.00

0.5-2.5

≤1.00

Al

≤0.35

1-1.8

1-2

0.2-0.6

≤0.4

≤0.5

0.2-0.8

Ti

1.9-2.35

1.8-2.7

2-3

0.7-1.2

≤0.4

≤0.15

0.7-1.15

Cr

13.5-16

18-21

18-21

20-23

20-23

20.5-23

17-21

Nb

--

--

--

--

--

--

4.75-5.5

Mo

1-1.5

--

--

2-2.5

8-10

8-10

2.8-3.3

B

0.001-0.1

≤0.008

≤0.02

--

--

--

--

V

0.1-0.5

--

--

--

--

--

--

W

--

--

--

1.4-1.8

--

0.2-1

--

Zr

--

≤0.15

≤0.15

--

--

--

--

Pb

--

--

≤0.002

--

--

--

--

Ce

--

--

--

≤0.05

--

--

--

Size Range

Wire

0.5-7.5mm

Rod/Bar

8.0-200mm

Strip

(0.50-2.5)*(5-180)mm

Tube

custom made

Plate

custom made

Primary Applications of A-286 Alloy Strip

A-286 alloy strip is employed in several critical applications across various industries due to its superior strength and resistance properties:

  1. Aerospace Fasteners
    A-286 is a preferred choice for high-strength fasteners used in jet engines and airframes. These include bolts, screws, and nuts that require high shear and tensile strength (up to 160 ksi / 1100 MPa after aging) and reliable performance under thermal cycling.

  2. Turbine & Jet Engine Components
    The alloy’s creep resistance makes it ideal for turbine blades, discs, and casings, as well as afterburner parts and exhaust systems that experience high temperatures and oxidation.

  3. Industrial Gas Turbines & Power Generation
    Components like combustor liners, bolts, washers, and high-temperature valves benefit from A-286’s performance under extreme heat and pressure, especially in chemical and petrochemical industries.

  4. Automotive & Racing Exhaust Systems
    A-286 alloy strip is used in turbochargers, exhaust manifolds, and other high-performance components due to its resistance to thermal fatigue and its ability to reduce weight while maintaining durability.

A-286 Alloy Strip application field

A-286 Alloy Strip process

Why Choose A-286 Alloy Strip?

  • Cost-Effective Alternative to Nickel Alloys
    A-286 offers comparable high-temperature performance to nickel-based alloys like Inconel 718, but at a more affordable price, making it an ideal choice for cost-sensitive applications.

  • Improved Machinability
    Easier to machine than many nickel alloys, A-286 allows for reduced production time and costs without compromising on performance.

  • Reliable Performance in Extreme Conditions
    Trusted by industries such as aerospace and energy, A-286 is well-suited for critical components that must perform reliably under sustained heat and stress.

Available Forms & Customization

A-286 alloy strip is available in a range of forms to meet diverse engineering requirements:

  • Cold-Rolled Strips – Thin gauge for precision parts.

  • Hot-Rolled Plates & Bars – For heavy-duty applications.

  • Custom Sizes & Heat Treatments – Solution annealed or aged to suit specific needs.

Common Standards:

  • ASTM A453 (Grade 660) – For bolting applications.

  • AMS 5525 / AMS 5731 – Aerospace material specifications.

A-286 Alloy Strip testing equipment

Recommended Products

OEM Services

ABOUT US
About DLX ALLOY

CHANGZHOU DLX ALLOY CO, LTD was established in 2002 and has got ISO9001 International Quality Management System Certificate and SGS Certificate. Our factory is professional in researching and producing special alloy material. From melting, drawing, heat treatment, finishing and testing .We offer nickel based, copper-based, and iron-based alloys, including super alloy, welding materials, anti-corrosion alloy, Precision Alloy , FeCrAl alloy, NiCr alloy, CuNi alloy, thermocouple and etc, in the form of wire, strip, ribbon, bar, tube, plate.

CHANGZHOU DLX ALLOYCHANGZHOU DLX ALLOYCHANGZHOU DLX ALLOY

About Our factory

Our 12,000㎡ factory is equipped with complete capabilities for research, production, testing, and packaging. We strictly adhere to ISO 9001 standards in our production processes, with an annual output of 1,200 tons. This ensures that we meet both quantity and quality demands. Furthermore, all products undergo rigorous simulated environment testing including high temperature, high pressure, and corrosion tests before being dispatched, ensuring they meet customer specifications. We also provide chemical analysis reports for every FeCrAl alloy, NiCr alloy, and other products purchased.

For all our clients, we offer timely and multilingual after-sales support and technical consulting, helping you resolve any issues swiftly and efficiently.

CHANGZHOU DLX ALLOY

Client Visits

Building Stronger Partnerships

CHANGZHOU DLX ALLOY

We support all kinds of testing:

CHANGZHOU DLX ALLOY

FAQ:

Q:What is the brand name of the high-temperature alloy product?
A:The brand name of the product is DLX.

Q:What is the model number of the high-temperature alloy product?
A: The model number of the product is High Temperature Alloy.

Q:Where is the product made?
A:The product is made in China JiangSu.

Q:What is the expected delivery time for the product?
A:The expected delivery time for the product is 7-10 days.

  • Click refresh picture
Top
×
Quote

Get the best price

We provide the best prices and services

×