The following are the average coefficient of expansion properties after annealing in hydrogen for 1 hr at 1650°F (900°C) and 15 minutes at 2010°F (1099°C) and cooled to room temperature within 1 hr. Material heat treated using this procedure should not exhibit any transformation when cooled to -112°F (-80°C) for 4 hrs. This was determined by means of metallographic examination.
Mean coefficient of thermal expansion as annealed.
Temperature | Coefficient | ||
77°F to | 25°C to | 10(-6)/°F | 10(-6)/°C |
212 392 572 662 752 842 932 1112 1292 1472 1652 | 100 200 300 350 400 450 500 600 700 800 900 | 3.25 2.89 2.85 2.72 2.81 2.92 3.41 4.34 5.06 5.73 6.25 | 5.86 5.20 5.13 4.89 5.06 5.25 6.15 7.80 9.12 10.31 11.26 |
Chemical composition